Following welding, for each parametric combination the samples are assessed by two different means:a visual inspection used to monitor the consistency of the welds and look for evidence of thermaldecomposition and a destructive test to determine the force required to fail the weld. As arepresentative value for the destructive test, the average maximum failure force F of four replicas wasused.